AWS E309L-16 Stainless steels Manu-manong electrode weld fabrication jointing
Application&Standard&Tandaan:
1. Angkop PARA SA STAINLESS STEEL AT CARBON STEEL O LOW ALLOY steel DISSimilar STEEL WELDING, STAINLESS steel composite plate cladding WELDING, 308 SERIES STAINLESS STEEL SURFACING WELDING sa carbon steel o mababang alloy na BAKAL.
2. Ang pamantayang naabot namin: GB/T983 E307-16, AWS A5.4 E307-16 & A5.4M E307-16, ISO3581-A:E(18 9 Mn Mo) R 1 2, ISO3581-B:ES307- 16
Aplikasyon: GINAMIT PARA SA PAREHONG URI NG STAINLESS steel na istraktura, composite steel at dissimilar steel na mga bahagi sa synthetic fiber, petrochemical at iba pang kagamitan sa pagmamanupaktura, maaari ding gamitin para sa nuclear reactor, pressure vessel inner wall transition layer surfacing at tower inner component welding.
Mga tampok
1. Titanium calcium hindi kinakalawang na asero elektrod, ang pangunahing komposisyon ay 22% CR-12%Ni;
2. Matatag na arko, magandang porma, pinong ripples, kaunting splashes, madaling de-slagging, magandang paglaban sa sunog ng balat ng droga, magandang stomatal resistance.
3. Ang weld metal ay naglalaman ng mas maraming ferrite at may mababang crack sensitivity.
Titanium calcium type ultra-low carbon Cr23Ni13 stainless steel electrode, ay maaaring gamitin para sa parehong AC at DC, nang walang niobium, titanium at iba pang matatag na elemento ng kemikal ay maaari ring labanan ang intercrystalline corrosion na dulot ng carbide precipitation. Ginagamit sa hindi kinakalawang na asero, composite steel at hindi magkatulad na bakal, tulad ng sintetikong hibla, petrochemical at iba pang kagamitan.
Paghahanda bago hinang:
Ang elektrod ay kailangang 300~350 ℃ para sa 1 oras na pagpapatayo, matinding oras ng kahalumigmigan upang magbigay ng mataas na temperatura ng pagpapatuyo sa 350 ℃ o naaangkop na extension ng oras ng pagpapatuyo, at pagpapatayo ng stacking layer hangga't maaari ay hindi hihigit sa 3 layer; Sikaping gamitin sa pagpapatuyo o ilagay sa electric insulation bucket nang hindi hihigit sa 2 araw upang makatipid, iwasan ang hindi kinakailangang pangalawang pagpapatuyo, upang maiwasan ang electrode coating off.
Kumpanya at Pabrika
Ang komposisyon ng produkto at pagpapakilala ng mga mekanikal na katangian
COMPONET NG KEMIKAL:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
MGA TUNTUNIN ng GB/T | 0.04 | 0.5-2.5 | 1.00 | 22.0-25.0 | 12.0-14.0 | 0.75 | 0.040 | 0.03 | 0.75 |
MGA PANUNTUNAN ng AWS | 0.04 | 0.5-2.5 | 1.00 | 22.0-25.0 | 12.0-14.0 | 0.75 | 0.040 | 0.03 | 0.75 |
HALIMBAWA VALUE | 0.028 | 0.95 | 0.8 | 24.4 | 13.1 | 0.32 | 0.027 | 0.004 | 0.05 |
MECHANICAL PROPERTY:
ARI-ARIAN | LAKAS NG YIELD(MPa) | LAKAS NG EXTENSION(MPa) | HEATTREAMENT℃xh | IMAPACT VALUE J/℃ | PAGPAPAhaba(%) | |||||||||
MGA TUNTUNIN ng GB/T | - | 510 | - | - | 25 | |||||||||
MGA PANUNTUNAN ng AWS | - | 520 | - | - | 30 | |||||||||
HALIMBAWA VALUE | - | 590 | - | - | 38 |
INIREREKOMENDADONG MGA PARAMETER SA PAGWALA:
DIAMETERS SPECIFICATIONS(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||||
KURYENTE (Amp) | H/W | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |
MGA DETALYE NG PAG-pack:
SEPCIFICATION | HABA | PCS/1KG | TIMBANG/1KG | |||
2.0mm | 300mm | 79PCS | 2KG | |||
2.6mm | 300mm | 48PCS | 2KG | |||
3.2mm | 350mm | 27PCS | 5KG | |||
4.0mm | 350mm | 16PCS | 5KG | |||
5.0mm | 350mm | 12PCS | 5KG |
TANDAAN:
H/W: pahalang na posisyong hinang
O/W: over-head position welding
Mga Karaniwang Kaso
Sertipiko
Ang komposisyon ng produkto at pagpapakilala ng mga mekanikal na katangian
COMPONET NG KEMIKAL:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
MGA TUNTUNIN ng GB/T | 0.04 | 0.5-2.5 | 1.00 | 22.0-25.0 | 12.0-14.0 | 0.75 | 0.040 | 0.03 | 0.75 |
MGA PANUNTUNAN ng AWS | 0.04 | 0.5-2.5 | 1.00 | 22.0-25.0 | 12.0-14.0 | 0.75 | 0.040 | 0.03 | 0.75 |
HALIMBAWA VALUE | 0.028 | 0.95 | 0.8 | 24.4 | 13.1 | 0.32 | 0.027 | 0.004 | 0.05 |
MECHANICAL PROPERTY:
ARI-ARIAN | LAKAS NG YIELD(MPa) | LAKAS NG EXTENSION(MPa) | HEATTREAMENT℃xh | IMAPACT VALUE J/℃ | PAGPAPAhaba(%) | |||||||||
MGA TUNTUNIN ng GB/T | - | 510 | - | - | 25 | |||||||||
MGA PANUNTUNAN ng AWS | - | 520 | - | - | 30 | |||||||||
HALIMBAWA VALUE | - | 590 | - | - | 38 |
INIREREKOMENDADONG MGA PARAMETER SA PAGWALA:
DIAMETERS SPECIFICATIONS(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||||
KURYENTE (Amp) | H/W | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |
MGA DETALYE NG PAG-pack:
SEPCIFICATION | HABA | PCS/1KG | TIMBANG/1KG | |||
2.0mm | 300mm | 79PCS | 2KG | |||
2.6mm | 300mm | 48PCS | 2KG | |||
3.2mm | 350mm | 27PCS | 5KG | |||
4.0mm | 350mm | 16PCS | 5KG | |||
5.0mm | 350mm | 12PCS | 5KG |
TANDAAN:
H/W: pahalang na posisyong hinang
O/W: over-head position welding