、Low-alloy steels Manu-manong electrode E8018-C1 weld fabrication makings
COMPONET NG KEMIKAL:
ALLOY(wt%) | C | Mn | Si | Ni | Cr | Mo | P | S |
MGA TUNTUNIN ng GB/T | 0.12 | 1.25 | 0.80 | 2.00-2.75 | - | - | 0.03 | 0.03 |
MGA PANUNTUNAN ng AWS | 0.12 | 1.25 | 0.80 | 2.00-2.75 | - | - | 0.03 | 0.03 |
HALIMBAWA VALUE | 0.055 | 0.85 | 0.32 | 2.2 | 0.023 | 0.11 | 0.007 | 0.006 |
MECHANICAL PROPERTY:
ARI-ARIAN | LAKAS NG YIELD(MPa) | LAKAS NG EXTENSION(MPa) | IMAPACT VALUE J/℃ | PAGPAPAhaba(%) | Paggamot ng init°Cxh | |||||
MGA TUNTUNIN ng GB/T | 460 | 550 | 27/-60 | 17 | 605*1 | |||||
MGA PANUNTUNAN ng AWS | 460 | 550 | 27/-60 | 19 | 605*1 | |||||
HALIMBAWA VALUE | 475 | 580 | 95/-60 | 26 | 605*1 |
INIREREKOMENDADONG MGA PARAMETER SA PAGWALA:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||
KURYENTE (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |
Iron powder low hydrogen potassium type hand electrode.
Dahil sa pagdaragdag ng pulbos na bakal, ang kahusayan sa pagkatunaw ay mas mataas, ang tibay ng epekto ng tinunaw na metal sa -60 ℃ na temperatura ng pagtatrabaho ay mahusay.
Matatag na arko, hindi gaanong splash, mahusay na pagbuo, madaling pag-alis ng slag, mahusay ang pagganap ng X-Ray.
Utility boiler
9,000 tonelada ng mga kemikal
Sanmen Nuclear Power Plant
COMPONET NG KEMIKAL:
ALLOY(wt%) | C | Mn | Si | Ni | Cr | Mo | P | S |
MGA TUNTUNIN ng GB/T | 0.12 | 1.25 | 0.80 | 2.00-2.75 | - | - | 0.03 | 0.03 |
MGA PANUNTUNAN ng AWS | 0.12 | 1.25 | 0.80 | 2.00-2.75 | - | - | 0.03 | 0.03 |
HALIMBAWA VALUE | 0.055 | 0.85 | 0.32 | 2.2 | 0.023 | 0.11 | 0.007 | 0.006 |
MECHANICAL PROPERTY:
ARI-ARIAN | LAKAS NG YIELD(MPa) | LAKAS NG EXTENSION(MPa) | IMAPACT VALUE J/℃ | PAGPAPAhaba(%) | Paggamot ng init°Cxh | |||||
MGA TUNTUNIN ng GB/T | 460 | 550 | 27/-60 | 17 | 605*1 | |||||
MGA PANUNTUNAN ng AWS | 460 | 550 | 27/-60 | 19 | 605*1 | |||||
HALIMBAWA VALUE | 475 | 580 | 95/-60 | 26 | 605*1 |
INIREREKOMENDADONG MGA PARAMETER SA PAGWALA:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||
KURYENTE (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |
Isulat ang iyong mensahe dito at ipadala ito sa amin