Nickel alloys Manu-manong electrode ENiCrMo-4 weld fabrication stuff
COMPONET NG KEMIKAL:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Fe | W | Mo | P | S | |
MGA TUNTUNIN ng GB/T | 0.02 | 1.00 | 0.20 | 14.5-16.5 | ≥55 | 4.0-7.0 | 3.0-4.5 | 15.0-17.0 | 0.02 | 0.015 | |
MGA PANUNTUNAN ng AWS | 0.02 | 1.00 | 0.20 | 14.5-16.5 | Margin | 4.0-7.0 | 3.0-4.5 | 15.0-17.0 | 0.04 | 0.03 | |
HALIMBAWA VALUE | 0.018 | 0.45 | 0.18 | 15.7 | 57.9 | 5.71 | 3.92 | 16.000 | 0.009 | 0.008 |
MECHANICAL PROPERTY:
ARI-ARIAN | LAKAS NG YIELD(MPa) | LAKAS NG EXTENSION(MPa) | IMAPACT VALUE J/℃ | PAGPAPAhaba(%) | ||||
MGA TUNTUNIN ng GB/T | 400 | 690 | - | 22 | ||||
MGA PANUNTUNAN ng AWS | - | 690 | - | 25 | ||||
HALIMBAWA VALUE | 570 | 770 | - | 40 |
INIREREKOMENDADONG MGA PARAMETER SA PAGWALA:
DIAMETERS SPECIFICATIONS(mm) | 2.6*300 | 3.2*350 | 4.0*350 | ||||||
KURYENTE (Amp) | H/W | 69-95 | 70-115 | 95-145 | |||||
O/W | 60-80 | 65-105 | 85-135 |
Mababang uri ng hydrogen na elektrod ng kamay, ang nominal na komposisyon (porsiyento ng timbang) ay 57Ni-16Mo-15.5cr-5.5Fe-4W-mababang C, nickel-chrome-molybdenum alloy electrode.
Napakahusay na paglaban sa kaagnasan, lalo na sa pitting corrosion at crack corrosion resistance.
Matatag na arko, magandang pagbubuo, maliit na splash, madaling pag-alis ng slag, magandang porosity resistance, ang mekanikal na katangian ng tinunaw na metal ay matatag.
Ang Tianshu Xing, isang malaking liquefied natural gas (LNG) carrier na may 174,000 cubic meters, ay itinayo bilang bow.
-
Sanmen Nuclear Power Plant
-
Hainan Huasheng phenol recovery tower
COMPONET NG KEMIKAL:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Fe | W | Mo | P | S | |
MGA TUNTUNIN ng GB/T | 0.02 | 1.00 | 0.20 | 14.5-16.5 | ≥55 | 4.0-7.0 | 3.0-4.5 | 15.0-17.0 | 0.02 | 0.015 | |
MGA PANUNTUNAN ng AWS | 0.02 | 1.00 | 0.20 | 14.5-16.5 | Margin | 4.0-7.0 | 3.0-4.5 | 15.0-17.0 | 0.04 | 0.03 | |
HALIMBAWA VALUE | 0.018 | 0.45 | 0.18 | 15.7 | 57.9 | 5.71 | 3.92 | 16.000 | 0.009 | 0.008 |
MECHANICAL PROPERTY:
ARI-ARIAN | LAKAS NG YIELD(MPa) | LAKAS NG EXTENSION(MPa) | IMAPACT VALUE J/℃ | PAGPAPAhaba(%) | ||||
MGA TUNTUNIN ng GB/T | 400 | 690 | - | 22 | ||||
MGA PANUNTUNAN ng AWS | - | 690 | - | 25 | ||||
HALIMBAWA VALUE | 570 | 770 | - | 40 |
INIREREKOMENDADONG MGA PARAMETER SA PAGWALA:
DIAMETERS SPECIFICATIONS(mm) | 2.6*300 | 3.2*350 | 4.0*350 | ||||||
KURYENTE (Amp) | H/W | 69-95 | 70-115 | 95-145 | |||||
O/W | 60-80 | 65-105 | 85-135 |